| Polypropylene impact copolymer. Titanpro 7523 is an intermediate impact material which complies with the U.S. Food and Drug Administration (FDA) regulation as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. TSCA Registry: CAS# 9010-79-1 Applications: Automotive parts, battery casing, appliances, housewares, seating, jerrycan caps. Advantages: Superior balance of properties; Good low temperature impact resistance; Excellent heat stability Fabrication: Equipment – ram or screw molding machine; Techniques - standard processing Information provided by Lotte Advanced Materials. |