BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to fill voids and bonding areas. Bonds well to a variety of substrates and materials, formulated especially to plastics, metals and elastomers. Perfect for bonding rough and irregular surfaces and applications requiring up to 15 seconds of alignment and work time. BONDING SCHEDULES: Steel: 25-35 seconds, ABS: 10-30 seconds, Neoprene: <5 seconds, PVC: 10-30 seconds, Aluminum: 10-20 seconds, Phenolics: 10-15 seconds, Polycarbonate: 15-20 seconds, Nitrile Rubber: 5-7 seconds.Information provided by BCC Products, Inc. |