MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Envalior ForTii® WX11-FC PPA-GF30 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® WX11-FC has excellent hydrolysis resistance, processability and surface quality and is ideal for complex and thin walled food and water contact applications. Features: USP class VI classified. Drinking Water Grade. 30% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors:
Available Properties
  • Density, ISO 1183, Dry
  • Moisture Absorption, Sim. to ISO 62, Dry
  • Linear Mold Shrinkage, Flow, ISO 294-4, Dry
  • Linear Mold Shrinkage, Transverse, ISO 294-4, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Cond
  • Tensile Strength at Break, ISO 527-1/-2
  • Tensile Strength at Break, ISO 527-1/-2
  • Tensile Strength at Break, ISO 527-1/-2
  • Tensile Strength at Break, ISO 527-1/-2, Cond
  • Tensile Strength at Break, ISO 527-1/-2
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Cond
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Cond
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Cond
  • Elongation at Break, ISO 527-1/-2, Cond
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2, Cond
  • Tensile Modulus, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2, Cond
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Tensile Modulus, ISO 527-1/-2, Cond
  • Tensile Modulus, ISO 527-1/-2, Cond
  • Flexural Strength, ISO 178, Cond
  • Flexural Strength, ISO 178, Dry
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178, Dry
  • Flexural Modulus, ISO 178, Cond
  • Charpy Impact Unnotched, ISO 179/1eU, Cond
  • Charpy Impact Unnotched, ISO 179/1eU, Cond
  • Charpy Impact Unnotched, ISO 179/1eU, Dry
  • Charpy Impact Unnotched, ISO 179/1eU, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Cond
  • Charpy Impact, Notched, ISO 179/1eA, Cond
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Volume Resistivity, IEC 62631-3-1, Dry
  • Volume Resistivity, IEC 62631-3-1, Cond
  • Dielectric Strength, IEC 60243-1, Dry
  • Dielectric Strength, IEC 60243-1, Cond
  • Comparative Tracking Index, IEC 60112, Dry
  • CTE, linear, ASTM D696
  • CTE, linear, Parallel to Flow, ASTM D696
  • Melting Point, ISO 11357-1/-3, 10°C/min. Dry
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2, Dry
  • Flammability, UL94, IEC 60695-11-10, Dry
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Envalior, former LANXESS

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.