PBT functional compound, electrically conductive Properties: dimensionally stable, electrically conductive, good chemical resistance, good aging behavior, high continuous used temperature, High strength, High stiffness, semi-crystalline Typical areas of application: Housing, Sliding elements, Bearing bushes, Structural components Industries: Automotive, Railroad industry, Electrical and electronics industry, Industry, Agriculture, Mechanical Engineering, Furniture industry, Sports & Recreation Information provided by BARLOG plastics GmbH. |