MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Corning ULE® 7973 Standard Grade Ultra Low Expansion Glass
Categories: Ceramic; Glass; Optical

Material Notes: 7973 is a titania-silicate low expansion glass that has been tailored to meet the needs for mask and optical substrates for EUVL applications. 7973 has a similar composition to ULE® 7972 glass and is made using the same flame deposition process. The lithography transition from 193nm to 13.4nm required a major design shift in stepper optics from refractive to reflective. In reflective optics, substrate materials should be purely passive. The incident light should reflect off of the multilayer coatings of the optics and the photomask without the introduction of any mechanical or optical distortion caused by the underlying substrate. To minimize distortion from the minute temperature changes and meet the stringent EUVL specifications, the substrates must have a near-zero coefficient of thermal expansion (CTE) and tightly controlled zero cross over range.

Excellent resistance to weathering. Exhibits virtually no surface clouding or electrical surface leakage when subjected to attack by water, sulfur dioxide, and other atmospheric gases. High resistance to attack by nearly all chemical agents.

ULE® 7973 comes in several grades with varying size/levels of inclusions and striae; CTE control, and birefringence. The distinguishing attributes of the Standard Grade are larger dimensions available.

Information provided by Corning Incorporated.

Vendors:
Available Properties
  • Density
  • Hardness, Knoop, kg/mm² at 200g load
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Bulk Modulus
  • Poissons Ratio
  • Shear Modulus
  • Volume Resistivity, 100Hz
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Specified mean from 5 to 35°C
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • CTE, linear, Approximate Instantaneous Value
  • Specific Heat Capacity
  • Thermal Conductivity
  • Softening Point
  • Annealing Point
  • Strain Point
  • Abbe Number, vd
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Corning Incorporated

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.