MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Parker Chomerics CHO-FAB CFT Shielding Tape
Categories: Polymer; Adhesive; Tape

Material Notes: Conductive Adhesive Nickel-Plated Fabric

Description: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape is extremely strong and lightweight, and has excellent conformability/wrapability to enhance shielding performance and appearance. Use of corrosion resistant nickel-plated cloth and Chomerics’ superior metal-particle-filled conductive adhesive technology produces a tape used in a wide variety of EMI shielding and grounding applications.

Typical Applications: Provide a low impedance connection between a braided cable shield and the metal connector backshell in molded cables. An effective EMI shielded assembly can be achieved without soldering the tape to the braid or backshell; EMI radiation measurement troubleshooting, using CHO-FOIL tape to shield ventilation slots or seam gaps; Provide electrical continuity in seams of EMI shielded rooms and electronic enclosures; Supply electrical contact to surfaces that can’t be soldered to, such as conductive plastic or aluminum; EMI shield for cables by wrapping the tape around the cable. An overlap is recommended; ESD shielding; Provide corrosion-resistant ground contact points; Fabric tape available where weight and flexibility are important, such as for wrapping cables.

Information provided by Chomerics

Vendors:
Available Properties
  • Thickness, Adhesive thickness
  • Thickness, Fabric thickness
  • Thickness, Total
  • Peel Strength, ASTM D1000, Initial
  • Peel Strength, ASTM D1000, 95% RH
  • Peel Strength, ASTM D1000
  • Peel Strength, ASTM D1000
  • Peel Strength, ASTM D1000, Salt fog corrosion
  • Taber Abrasion, mg/1000 Cycles, CHO-TP-57, 500 gram weight. CS-10 wheel
  • Surface Resistance, CHO-TP-57, Initial Surface Resistivity (SR)
  • Surface Resistance, CHO-TP-57, Initial through resistivity (TR)
  • Surface Resistance, CHO-TP-57, Initial Taber Abrasion
  • Surface Resistance, CHO-TP-57, 95% RH; (SR)
  • Surface Resistance, CHO-TP-57, 95% RH; (TR)
  • Surface Resistance, CHO-TP-57, (SR)
  • Surface Resistance, CHO-TP-57, (SR)
  • Surface Resistance, CHO-TP-57, (TR)
  • Surface Resistance, CHO-TP-57, (TR)
  • Surface Resistance, CHO-TP-57, Salt fog corrosion; (SR)
  • Surface Resistance, CHO-TP-57, Salt fog corrosion; (TR)
  • Surface Resistivity per Square, MIL-STD-202C, [ohm/in2]; <.016 ohm/cm2
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.