MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Zell-Metall Engineering Plastics Zellamid 1200 G  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material with high molecular weight, high crystallinity and very low inner stress level. Zellamid® 1200 G is showing significant low moisture absorption, superior dimensional stability combined with high impact strength even at low temperatures and an excellent chemical resistance.

Zellamid® 1200 G is the ideal longterm solution for bushes, bearings, rollers and gear wheels subjected to high load and wear demanding for dimensional stability particularly when exposed to high humidity and water.

Vendors:
Available Properties
  • Density
  • Moisture Absorption at Equilibrium, 50% RH
  • Water Absorption at Saturation, 23°C
  • Hardness, Shore D, DIN 53505
  • Ball Indentation Hardness, DIN 53456
  • Tensile Strength at Break, DIN 53455
  • Elongation at Break, DIN 53455
  • Tensile Modulus, DIN 53457
  • Charpy Impact Unnotched, DIN 53453
  • Charpy Impact, Notched, DIN 53453
  • Coefficient of Friction, to steel, added lubrication
  • Coefficient of Friction, ISO/DTR 7147, to steel, no lubrication
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, DIN 52612
  • Melting Point
  • Maximum Service Temperature, Air, long time operation
  • Maximum Service Temperature, Air, medium time operation
  • Maximum Service Temperature, Air, a few hours operation
  • Minimum Service Temperature, Air
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.