MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Microtherm Group Steelflex Panel Filament Reinforced Silica Thermal Insulation Panel, Water Repellent
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Steelflex Panels are a cost effective alternative to fully hydrophobic insulation panels where water may be present during installation. A polyethylene film covering allows the panels to rest in contact with wet castable cement without detriment to the thermal performance.
    Properties
  • Water repellent high temperature thermal insulation for steel making applications.
  • Stable thermal performance for continuous exposure to 1000°C (1832°F).
  • Formulation based on pyrogenic silica with a mineral oxide opacifier and E-glass filament reinforcement.
  • Non-combustible microporous insulation core.
  • Environmentally friendly.
  • Free of harmful respirable fibers.
    Benefits
  • Water repellent high temperature insulation.
  • Ultra thin allowing productive volume savings.
  • Clean in use.
  • Fast, simple installation.
  • Extremely cost effective thermal solutions.

Information provided by Microtherm.

Vendors:
Available Properties
  • Density
  • Thickness
  • Compressive Strength, ASTM C165, Resistance at 10%, 300 kg/m³
  • Compressive Modulus, ASTM C165, @ 300 kg/m³
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Thermal Conductivity, ASTM C177, ISO 8302, @ 320 kg/m³
  • Maximum Service Temperature, Air, for long term exposure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.