MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP30LTE Low Thermal Expansion, Dimensionally Stable Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Room temperature curing
  • Low viscosity
  • Low shrinkage upon cure
  • Very low coefficient of expansion
  • Superior dimensional stability
  • Serviceable from -100°F to +250°F
Product Description: Master Bond EP30LTE is a specialty epoxy system featuring an exceptionally low coefficient of thermal expansion (CTE). Also noteworthy is its superior dimensional stability. It can be used in bonding, coating, sealing and encapsulation applications. This lower viscosity system will cure at room temperature or more quickly at elevated temperatures. To optimize the properties, it is recommended to cure at room temperature for 12-24 hours, followed by a post cure of a few hours at 150-200°F. The CTE is in the range of 15-18 x 10-6 in/in/°C; markedly lower than other systems. Additionally, it has good thermal conductivity and is highly electrically insulative. Its linear shrinkage upon curing is exceptionally low, less than 0.01%. EP30LTE bonds well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. It is 100% reactive and does not contain any solvents or diluents. This system offers excellent resistance to many chemicals, such as water, fuels and oils, as well as a number of acids and bases. It is serviceable over the wide temperature range of -100°F to +250°F. Part A of this system is off white in color and Part B is clear. Master Bond EP30LTE is especially used in aerospace, optical, electronic, specialty OEM and other applications where an ultra low CTE along with dimensional stability is desirable.

Product Advantages:

  • 100% reactive, contains no diluents or solvents
  • Very low shrinkage upon cure
  • Lower viscosity; good flow properties — ideal for small to moderate sized castings
  • Exceptionally low thermal expansion coefficient: about 15-18 x 10-6 in/in/°C
  • Good thermal conductivity while still electrically insulative
  • Superior dimensional stability

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.