MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemours Krytox™ 240AA PFPE Aerospace Grade Fluorinated Grease, Aerospace Grease Grade
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Many grades and special formulations of Krytox™ oils and greases offer superior performance characteristics and certifications for aerospace applications. They operate effectively in high vacuum and extreme temperatures, and are able to endure exposure to fuels, oxidizers, and radiation.

Features:

  • Unaffected lubricity and viscosity within a wide temperature range
  • Stable physical properties over time, including radiation resistance
  • Virtually unaffected by harsh environments and caustic chemicals
  • Resistant to vapor loss in a vacuum (e.g., during high-altitude orbit or deep space flight)
  • Long wear and low-energy consumption due to excellent friction-reducing characteristics
  • Compatible for use with most metals, elastomers, plastics, paints, and finishes,
  • Nontoxic, nonflammable, inert, and non-evaporative.

Information provided by Chemours Krytox

Vendors:
Available Properties
  • Density, grease
  • Volatiles, ASTM D2595, wt% loss
  • Viscosity Measure, ASTM D445, base oil
  • Viscosity Measure, ASTM D445, base oil
  • Viscosity Measure, ASTM D445, base oil
  • Viscosity Measure, ASTM D445, base oil
  • Vapor Pressure, Knudsen, base oil
  • Vapor Pressure, Knudsen, base oil
  • Penetration, ASTM D217, 60 strokes
  • Oil Separation, ASTM D6184, wt% loss
  • Oil Separation, ASTM D6184, wt% loss
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point, ASTM D97
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont Performance Lubricants

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.