PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PEARLCOAT® 163K is used in melt coatings on textile substrates, for end-uses in industrial coatings (for life-jackets, etc.) obtained by extrusion and calendering.All information provided by Merquinsa |