MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ChevronTexaco Havoline® SAE 10W-30 Synthetic Motor Oil
Categories: Fluid; Lubricant

Material Notes: Havoline Synthetic Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, sport utility vehicles, and light trucks. 5W-30 and 10W-30 meet:
  • API Service Categories SL/CF, SJ/CF, SH, SG, Energy conserving for API SL
  • ILSAC GF-3
  • ACEA A1-98
  • General Motors GM 9986125, 9986126, 9986137, 4718M
  • Chrysler MS 6395-H
  • Ford ESE-M2C 153-G
  • Japanese VTW
  • Peugeot TU 3M Scuff Test
  • Department of Defense Commercial Item Description A-A-52309B

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222101; MSDS Number: 8602

Vendors:
Available Properties
  • API Gravity
  • Viscosity, Cold Crank
  • Viscosity Measurement, Viscosity Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, Sulfated Ash
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point
  • Phosphorus, P
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.