MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Go Yen Chemical Adhesive Agent Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Can provide adhesive agent long-term fireproof effect.
  • Through the only special Nano technology in Asia, resin can be formed with excellent flame retard structure.
  • Without volatility and it is compatible to most of macromolecular compound.
  • Can enhance the additional value of various synthetic resin.
  • With high heat-stability.
  • Especially for adhesive agent.
  • With special Nano structure, it can be added in various resin directly and form a kind of Nano flame retard surface.
Applications:
  • Can apply on various adhesive agents.
  • EPOXY
  • thermosetting resin such as phenolic resin, acrylic, epoxy, unsaturated resin, polyester resin, acrylic resin etc.
  • Coating and various resin application such as flame retard coating, all kinds of acrylic related products, PU, PMMA, latex resins and adhesives.
  • Thermoplastic : TPU, PVC, PP, POLYOLIFIN, PET, NYLON, POM, engineering plastics.
  • Rubber industrial: EPDM, CR, NBR, SBR, SIR, CSM, NR.IIR, and all kinds of fireproof rubber
  • Elastomers:TPE, TPU, SBS, SEBS, TPR, TPV and all kinds of elastomers.
  • Foam polymer: can apply on many compound foam application, especially on flexible and rigid PU foam, EVA foam material, EPS foam.
  • Other application: ink, paper making, furniture plywoods, pigment, fireproof masterbatch, textile and various fireproof electronic products.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Particle Size
  • Acid Value, mgKOH/g
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.