MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ductile Iron torsion grade 60-40-18
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: The listed composition represents possible constituent elements in 60-40-18. Most ductile irons are specified by mechanical properties and have loosely defined compositions. For example, 60-40-18 ductile iron is specified to have a minimum tensile strength of 60 ksi (414 MPa), a yield strength of 40 ksi (276 MPa) and an elongation of 18%. Copper, nickel, and molybdenum are often added to ductile irons to improve strength and hardenability. Determined for a single temperature of ductile iron, heat treated to approximate various standard grades. Properties were obtained using test bars machined from 25 mm keel blocks.

Corrosion Resistance: Copper and nickel, along with chromium and additional amounts of silicon can improve corrosion resistance.

Vendors:
Available Properties
  • Density, Typical value of ductile iron
  • Hardness, Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Vickers, Approximated. Converted from Brinell hardness.
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Carbon, C, Total carbon
  • Cerium, Ce
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.