MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hanwha Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDELĀ® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This composite material exhibits highly oriented material properties in the longitudinal direction of the oriented glass fibers. This material is typically used in semi-structural applications where high material properties in one direction are desired, such as automotive bumper beams.

Mechanical properties and mold shrinkage measured on flat plaques.

Information provided by Azdel.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792, Laminate
  • Specific Gravity, ASTM D792, Molded
  • Filler Content, Internal, By weight (ashing)
  • Thickness, Internal, Sheet
  • Linear Mold Shrinkage, ASTM D955, Measured on flat plaques
  • Tensile Strength at Break, ISO 527, Transverse direction
  • Tensile Strength at Break, ISO 527, Longitudinal direction
  • Elongation at Break, ISO 527, Transverse direction
  • Elongation at Break, ISO 527, Longitudinal direction
  • Tensile Modulus, ISO 527, Transverse direction
  • Tensile Modulus, ISO 527, Longitudinal direction
  • Flexural Strength, ISO 178, Transverse direction
  • Flexural Strength, ISO 178, Longitudinal direction
  • Flexural Modulus, ISO 178, Transverse direction
  • Flexural Modulus, ISO 178, Longitudinal direction
  • Poissons Ratio, ISO 527, Transverse direction
  • Poissons Ratio, ISO 527, Longitudinal direction
  • Izod Impact, Notched, ISO 180, transverse direction
  • Izod Impact, Notched, ISO 180, longitudinal direction
  • Impact, ASTM D3763, Multi-axial in kg, at max. load
  • Impact Test, ASTM D3763, Multi-axial, at max. load
  • Impact Test, ASTM D3763, Multi-axial, at failure
  • CTE, linear, ASTM E831, longitudinal direction
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Transverse direction
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Longitudinal direction
  • Flame Spread, FMVSS302, longitudinal direction
  • Flame Spread, FMVSS302, transverse direction
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.