Temper: Spring Fabrication Properties: Good Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Capacity for Being Cold Worked; Fair Suitability – Soldering, Brazing, Oxyacetylene Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed |