MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Solvay Toolcoat 805 Adhesive tape
Categories: Polymer; Adhesive; Tape

Material Notes: Description: Adhesive tape. Ideally suited for tool surface release applications.

Features & Benefits:

  • TOOLCOAT 805 is a Tetrafluoroethylene (TFE) impregnated fiberglass pressure sensitive tape, with a fully cured silicone adhesive (Toolcoat 805S), or acrylic adhesive (Toolcoat 805A).
  • Adheres to tool surface to provide multiple releases on all types of tooling surfaces
  • Also eliminates the need for liquid or paste release coating on tool surfaces that many be potential contamination problems, and is especially useful on composite tools and press platens.
  • TOOLCOAT 805 gives optimum release, low friction, electrical insulation, dimensional stability and temperature resistance
  • Other applications are flash control, heat-sealing machines, covering of coating and drying rolls, chute lining, linings for guide rails, and any other non-stick, low friction applications.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Thickness, Adhesive
  • Thickness, Fiberglass Tape
  • Thickness, Total
  • Maximum Service Temperature, Air, (intermittent) All Toolcoat Acrylic items
  • Maximum Service Temperature, Air, All Toolcoat Silicone items
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.