Production Method: Obtained by interaction of oleic acid and ethylene oxide. Application: Intended for use from 3% to 5% water emulsions as antistatic, lubricating and finishing agent for chemical fibers, natural and mixed fibers, as well as softener in the production of flax-fibers as a dispersing agent or emulsification agent for different dispersing media and as a degreaser in detergents. Information Provided by Kazanorgsintez |