MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Evonik Vestodur® CL2030 30% Glass Reinforced, Crosslinkable PBT Based Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: VESTODUR CL2030 is a 30 % glass fiber-reinforced, self-extinguishing compound for injection molding, based on modified polybutylene terephthalate (PBT).Moldings of VESTODUR CL2030 can be crosslinked by high-energy radiation (ß- or ?-radiation) or heat. The influence of the radiation to the mechanical properties is negligible. The short-term heat resistance is increased up to 400 °C depending on the conditions. Crosslinked parts of VESTODUR CL2030 can be used in common soldering processes like surge soldering, vapor phase soldering or IR soldering which are typical in the electronic industry. The incorporated flame retardant is non-migrating and has no corrosive effects on metal inserts or neighboring metal parts. Laser marking with high contrast is possible.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, sheet with film gate at rim, mold temperature 80°C
  • Linear Mold Shrinkage, Transverse
  • Melt Flow, ISO 1133
  • Ball Indentation Hardness, ISO 2039-1, H30 (350 Kgy)
  • Tensile Strength at Break, ISO 527-1/2
  • Elongation at Break, ISO 527-1/2
  • Tensile Modulus, ISO 527-1/-2
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • Tensile Creep Modulus, 1 hour, ISO 899-1, Uncrosslinked
  • Tensile Creep Modulus, 1 hour, ISO 899-1, Crosslinked
  • Tensile Creep Modulus, 1000 hours, ISO 899-1, Uncrosslinked
  • Tensile Creep Modulus, 1000 hours, ISO 899-1, Crosslinked
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, K20/P50
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Test Solution A CTI
  • Comparative Tracking Index, IEC 60112, 100 drops value
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 75-1/-2, Method B, 50 N
  • Vicat Softening Point, ISO 75-1/-2, Method A, 10 N
  • Flammability, UL94, IEC 60695
  • Flammability, UL94, IEC 60695
  • Flammability, UL94, IEC 60695
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.