MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Appeel® 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including polypropylene, polystyrene, and polystyrene foam and is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resins.

General Processing Information: The melt temperature of Appeel® 11D569 should be maintained in the 175-238°C (350-460°F) range. Selection of a specific melt temperature will depend on screw configuration, potential power limitations, and the need to match melt viscosities. However, melt temperatures above 238°C (460°F) should be avoided because of possible thermal degradation of the resin. If the process is stopped for short periods of time, the Appeel® resin extruder should be kept turning at low rpm. For a permanent shutdown, the Appeel® resin should be purged using an available polyethylene resin run at the same extrusion temperature used for the Appeel® resin. Making frequent changes in screw speed during shutdown and subsequent start-up will help remove the previous material from the machine more effectively.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Seal Strength, PP, bar temp 150-200°C
  • Seal Strength, HDPE, bar temp 150-200°C
  • Melting Point, Freezing Point via DSC/ASTM D3418
  • Melting Point, Upon Melting via DSC/ASTM D3418
  • Vicat Softening Point, ASTM D1525
  • Melt Temperature, Degrades above 238°C.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Packaging and Industrial Polymers

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.