Temper: Hard Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Butt Weld; Poor Suitability – Capacity for Being Hot Formed Common Fabrication Processes: Forming and Bending; Machining; Piercing and Punching Typical uses: Power and Pump Cylinder Liners; Power and Pump Cylinders; Primers; J Bends; Plumbing Accessories; Plumbing Brass Goods; Pump Lines; Trap Lines Applicable Specifications: Seamless Tube – ASME SB135; Tube – FEDERAL WW-T-791, SAE J461, AMS 4555, MILITARY MIL-T-46072, Seamless (Metric) ASTM B135/B135M, AMS 4554, ASTM B135, SAE J463 |