Characterization: Baynat 3002 polyurethane foam system is used in automotive headliner applications. Properties / Applications: The Baynat 3002 polyurethane system is supplied as two reactive liquid components. Component A is a polymeric diphenylmethane diisocyanate (MDI). Component B is a polyether polyol system. Baynat 3002 polyurethane foam system is used in automotive headliner applications. This system allows low weight, good thermal dimensional stability, and high definition of surface structure. As with any product, use of the Baynat 3002 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability. Information provided by Covestro |