  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tank liners, electrical insulation and low friction applications.

    Features and Benefits:
  • Excellent thermal stability
  • Excellent electrostatics
  • Excellent non-stick performance
  • Outstanding flow and fluidization
  • Excellent stress crack resistance
  • Smooth surfaces
  • Process targets: powder coating
  • Non-wetting
  • Heat resistant to 260°C (500°F)
  • Low friction
  • Good transparency
  • Chemical resistant

    This product complies with 21 CFR 177.1550 FDA regulations

Information provided by the Dyneon division of 3M.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Bulk Density, DIN 53466
  • Particle Size
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790
  • Melting Point, ASTM D4591
  • Maximum Service Temperature, Air
  • Oxygen Index, ASTM D2863
  • Transmission, Visible, transparent, but thickness not quantified
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dyneon, Division of 3M

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.