Description: AKROTEK® PEEK CF 40 black (5099) is a 40 % carbon fibre reinforced polyetheretherketone with high flexural strength and good sliding properties Applications: Applications are mainly elements in the automotive-, aeronautical-, industrial- and medical engineering that require high strength and high stiffness in a temperature environment above 150 °C Information provided by Akro-Plastic GmbH |