MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Jewelry bronze, UNS C22600, OSO15 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot workability for blanking, coining, drawing, piercing and punching, shearing, spinning, squeezing and swaging, stamping, heading and upsetting, roll threading and knurling.

Applications: angles, channels, chains, fasteners, costume jewelry, lipstick cases, compacts, base for gold plate.

Test specimen: flat products - 1mm thickness.

Key Words: CA226
Vendors:
Available Properties
  • Density
  • Grain Size, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Grain Size, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Grain Size, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Grain Size, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Grain Size, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Hardness, Rockwell F
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Tensile Strength, Ultimate, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Tensile Strength, Ultimate, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Tensile Strength, Ultimate, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Tensile Strength, Ultimate, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Tensile Strength, Yield
  • Elongation at Break, In 50 mm
  • Elongation at Break, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Elongation at Break, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Elongation at Break, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Elongation at Break, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Elongation at Break, strip with initial grain size of 0.035 mm, cold rolled 50% to 1 mm thick, annealed 1h
  • Modulus of Elasticity
  • Poissons Ratio
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Annealing Temperature
  • Hot-Working Temperature
  • Recrystallization Temperature, Approximately, for 1mm
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.