Good to excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, drawing, bending, heading, and upsetting, shearing, roll threading, knurling and stamping. Applications: bellows, bourdon tubing, clutch discs, cotter pins, diaphragms, fasteners, lock washers, wire brushes, chemical hardware, textile machinery, welding rod. Trace content of Phosphorus.Test specimen: flat products - 1mm thickness. |
CDA 510, PB102, ISO CuSn5 |