MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Overview of materials for 2000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "2000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors:
Available Properties
  • Density, Average value: 2.79 g/cc Grade Count:190
  • Hardness, Brinell, Average value: 114 Grade Count:70
  • Hardness, Knoop, Average value: 147 Grade Count:55
  • Hardness, Rockwell A, Average value: 46.5 Grade Count:52
  • Hardness, Rockwell B, Average value: 73.7 Grade Count:55
  • Hardness, Vickers, Average value: 135 Grade Count:55
  • Tensile Strength, Ultimate, Average value: 405 MPa Grade Count:119
  • Tensile Strength, Yield, Average value: 309 MPa Grade Count:119
  • Elongation at Break, Average value: 8.85 % Grade Count:119
  • Creep Strength, Average value: 383 MPa Grade Count:3
  • Rupture Strength, Average value: 452 MPa Grade Count:3
  • Modulus of Elasticity, Average value: 76.3 GPa Grade Count:119
  • Compressive Yield Strength, Average value: 397 MPa Grade Count:7
  • Compressive Modulus, Average value: 75.2 GPa Grade Count:14
  • Notched Tensile Strength, Average value: 393 MPa Grade Count:5
  • Ultimate Bearing Strength, Average value: 786 MPa Grade Count:7
  • Bearing Yield Strength, Average value: 508 MPa Grade Count:7
  • Poissons Ratio, Average value: 0.327 Grade Count:84
  • Fatigue Strength, Average value: 164 MPa Grade Count:43
  • Fracture Toughness, Average value: 31.7 MPa-m½ Grade Count:12
  • Machinability, Average value: 67.9 % Grade Count:29
  • Shear Modulus, Average value: 29.0 GPa Grade Count:83
  • Shear Strength, Average value: 248 MPa Grade Count:66
  • Electrical Resistivity, Average value: 0.00000492 ohm-cm Grade Count:89
  • CTE, linear, Average value: 22.8 µm/m-°C Grade Count:112
  • Specific Heat Capacity, Average value: 0.869 J/g-°C Grade Count:78
  • Thermal Conductivity, Average value: 139 W/m-K Grade Count:105
  • Melting Point, Average value: 573 °C Grade Count:73
  • Solidus, Average value: 529 °C Grade Count:73
  • Liquidus, Average value: 642 °C Grade Count:56
  • Annealing Temperature, Average value: 408 °C Grade Count:51
  • Solution Temperature, Average value: 510 °C Grade Count:58
  • Aging Temperature, Average value: 166 °C Grade Count:31
  • Aluminum, Al, Average value: 93.5 % Grade Count:184
  • Beryllium, Be, Average value: 0.00122 % Grade Count:5
  • Bismuth, Bi, Average value: 0.362 % Grade Count:33
  • Chromium, Cr, Average value: 0.0973 % Grade Count:93
  • Copper, Cu, Average value: 3.96 % Grade Count:184
  • Iron, Fe, Average value: 0.454 % Grade Count:173
  • Lead, Pb, Average value: 0.516 % Grade Count:32
  • Lithium, Li, Average value: 1.57 % Grade Count:27
  • Magnesium, Mg, Average value: 0.760 % Grade Count:170
  • Manganese, Mn, Average value: 0.431 % Grade Count:164
  • Nickel, Ni, Average value: 0.664 % Grade Count:28
  • Oxygen, O, Average value: 0.519 % Grade Count:4
  • Si+Fe, Average value: 0.675 % Grade Count:12
  • Silicon, Si, Average value: 0.443 % Grade Count:173
  • Silver, Ag, Average value: 0.397 % Grade Count:18
  • Tin, Sn, Average value: 0.610 % Grade Count:16
  • Titanium, Ti, Average value: 0.127 % Grade Count:145
  • Vanadium, V, Average value: 0.0833 % Grade Count:24
  • Zinc, Zn, Average value: 0.298 % Grade Count:179
  • Zirconium, Zr, Average value: 0.141 % Grade Count:62
  • Zr+Ti, Average value: 0.237 % Grade Count:4
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.