Description: G-510p is an expandable polystyrene grade, containing graphite, with reduced thermal conductivity. Pentane is used as a blowing agent. The product is delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1100 kg octabins. Applications: The properties of G-510p make it suitable for the production of light and heavy insulation board by block or shape moulding. Information provided by BEWi Synbra |