MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Momentive Performance Materials GE Silicones Enduris 3525 Silicone Roof Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: GE Enduris 3525 silicone roof coating is a high performing protective barrier for a variety of architectural surfaces and roofing substrates. Upon cure, Enduris 3525 silicone roof coating forms a durable, breathable and waterproof roofing membrane that is highly resistant to degradation from heat, cold, UV light, and natural weathering.

Features: Silicone Durability, Low VOC Formula, Ease of Use, High Build Formulation, Storage & Shelf Life.

Applications: For structurally sound roofing applications including over existing coatings, single ply, modified bitumen and BUR, foam, metal and other horizontal and vertical roofing. Perform an adhesion test on each surface type to verify adhesion.

Information provided by Momentive Performance Materials.

Vendors:
Available Properties
  • Solids Content, ASTM D1644-01 (Modified), By volume.
  • Solids Content, ASTM D1644-01 (Modified), By weight.
  • Volatile Organic Compounds (VOC) Content, EPA Method 24
  • Viscosity, ASTM D2196
  • Hardness, Shore A, ASTM D2370
  • Tensile Strength, ASTM D2370
  • Elongation at Break, ASTM D2370
  • Tear Strength, ASTM D624
  • Emissivity (0-1), ASTM C1371, Initial
  • Emissivity (0-1), ASTM C1371, Accelerated aging test by QUV
  • Reflection Coefficient, Visible (0-1), ASTM C1549, Solar Reflectance; Accelerated aging test by QUV
  • Reflection Coefficient, Visible (0-1), ASTM C1549, Solar Reflectance; Initial
  • Tack-Free Time, ASTM D3960
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.