KEBABLEND / H 36.1900 PPS is a functional compound based on PPS with high density. Properties: dimensionally stable, high continuous used temperature, High density Typical areas of application: Holding magnets, Magnets for sensors, Pumps and motors Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering Information provided by BARLOG plastics GmbH. |