MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SACO AEI PEXIDAN® HF V/T Moisture-curable Low Smoke Zero-Halogen (LSZH)
Categories: Polymer; Thermoplastic

Material Notes: Solar UV resistant, silane crosslinkable, Halogen Free, flame retardant compound for low-voltage building wire applications (VW-1 Rated – styles XHHW-2, RHW-2, RHH, and SIS)

PEXIDAN® HF V/T is a unique low smoke halogen-free flame retardant 90°C wet-rated XL-insulation system curable by moisture. It consists of a silane pre-grafted base compound SX653 and a catalyst masterbatch CM540U. Mixed and extruded in the proper proportions (95:5), the two components result in a material that is cross-linkable by exposure to 90°C hot water. PEXIDAN® HF V/T is REACH and RoHS-compliant. Wire made with PEXIDAN® HF V/T may be marked VW-1, as well as Oil Resistant “PR I” and “PR II”, Gas & Oil Resistant “GR I” and “GR II”, “-40C” and “SUNRES” in all colors.

Information provided by SACO AEI Polymers, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Deformation, UL 1581 / UL 2556
  • Storage Temperature
  • Tensile Strength at Break, UL 1581 / UL 2556
  • Tensile Strength at Break, UL 1581 / UL 2556, After 96 hours oil
  • Tensile Strength at Break, UL 1581 / UL 2556, After 60 day oil
  • Tensile Strength at Break, UL 1581 / UL 2556, after thermal ageing
  • Elongation at Break, UL 1581 / UL 2556
  • Elongation at Break, UL 1581 / UL 2556, After 96 hours oil
  • Elongation at Break, UL 1581 / UL 2556, after thermal ageing
  • Elongation at Break, UL 1581 / UL 2556, After 60 day oil
  • Tensile Set, SACO AEI DWI-QA-4007 based on ICEA T-28-562, Hot set after 41% elongation under load, 20N/cm2
  • Crush Resistance, UL 1581 / UL 2556
  • Dielectric Constant, UL 1581 / UL 2556, (SIC)
  • Dielectric Breakdown, UL 1581 / UL 2556, after glancing impact
  • Dielectric Breakdown, UL 1581 / UL 2556, initial
  • Smoke Density, ASTM E662, Non-flaming, Dsmax (corrected)
  • Smoke Density, ASTM E662, Flaming, Dsmax (corrected)
  • Smoke Density, ASTM E662, Flaming, Ds
  • Smoke Density, ASTM E662, Non-flaming, Ds
  • Oxygen Index, ASTM D2863
  • Processing Temperature, barrel zones
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.