MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Danquinsa DANTHANE® 125H Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANTHANE_ 125H is a polyester based, thermoplastic, aromatic structured TPU-granule. DANTHANE_ 125H has the distinction by its low softening point and its good adhesive behaviour. DANTHANE® 125H is applied by melt calander coating of textiles or other supporting materials. DANTHANE_ 125H is used at the production of coated textiles as they were needed for example at:
  • sealing of seams
  • membrane foils
  • mattress coatings
  • good thermic welded foils
  • ?thermobond equipment
> Application: DANTHANE_ 125H is needed by the hot melt coating of industrial textiles. Coated textiles or even produced mono foils distinguishes themselves by their excellent reactivation behaviour and thermic welding behaviour. DANTHANE_ 125H is further best suitable for thermobonding equipment of textiles. By this kind of application it is possible to extrude the granules of DANTHANE_ 125H into films. Grinded to powder there is the possibility to apply the powder of DANTHANE_ 125H by spread coating, powder or dot point coating. Concerning powder we refer to the type DANTHANE_ 125H–Powder.

Information provided by Danquinsa GMBH

Vendors:
Available Properties
  • Density, DIN 53.479
  • Viscosity, DIN 53.735
  • Brookfield Viscosity, 20% in THF, RVT, spindle 3, 20 U.p.M./20°C
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • Hardness, Shore A, DIN 53.505
  • Tensile Strength, DIN 53.504
  • Elongation at Break, DIN 53.504
  • 100% Modulus, DIN 53.504
  • 200% Modulus, DIN 53.504
  • 300% Modulus, DIN 53.504
  • Abrasion, DIN 53.516, [mm³]
  • Compression Set, DIN 53.517
  • Compression Set, DIN 53.517
  • Melting Point, Kofler
  • Softening Point, Kofler
  • Glass Transition Temp, Tg, DIN 51.007, DSC
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.