MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The grade has a martensitic microstructure. The final mechanical properties may be optimized by selecting an appropriate heat treatment. In the annealed conditions the alloy presents ductility and may be formed. Chromium additions (~13%) improve the corrosion resistance, particularly in wet conditions when compared to C-Mn steels. Slightly acidified and abrasion conditions are considered. The main applications concern mechanical industry, oil and gas industry, sugar industry and constructional components.

Information provided by manufacturer.

Key Words: EURONORM 1.4006 X12 Cr 13, AFNOR Z 12 C 13, DIN W 1.4006 (DIN 17440), ASTM A240 TP 410, UNS S41000
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Typical
  • Tensile Strength, Ultimate, Minimum Guaranteed
  • Tensile Strength, Yield, Minimum Guaranteed
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact, Typical Toughness (long)
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Groupe Arcelor

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.