A 15% mineral filled low-combustible polypropylene. This material displays high mechanical properties, low buckling and shrinkage parameters, it may be applied as a substitution of metals, thermosetting polymers and other thermoplastics (polyamides, polyester, ABS plastics) in technical products, including those exploited in chemically aggressive conditions, and general items. Designed for injection molding and extrusion of various items and parts for construction, electrical tools, machine engineering, household appliances, transportation and etc. Available in natural, white, light-grey, black and graphite.Information provided by Polyplastic Compounds |