Product Description: Tuflin™ HS-7098F NT 7 ethylene-hexene copolymer, LLDPE resin designed for cast and blown film applications such as trash bags, industrial can liners, and retail bags. Films extruded with HS-7098F NT 7 exhibit superb toughness, high tensile strength and elongation, excellent tear and puncture resistance, and are readily heat sealable. Main Characteristics: - Hexene Linear Low Density Resin
- Excellent toughness
- High strength
- Compiles with US FDA 21 CFR 177.1520©3.1a
Application: Heavy Duty Industrial and Consumer Liners Availability: North America Agency Ratings: FDA 21 CFR 177.1520(c)3.1a Additive: Antiblock: 5000 ppm; Processing Aid: No; Slip: 900 ppm Form: Pellets Processing Method: Blown Film Information provided by The Dow Chemical Company |