MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ChevronTexaco Miltex EP NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Texaco Miltex EP delivers value through:
  • Good water resistance — Strong resistance to wash out of bearings
  • Good rust and corrosion protection, even in wet conditions
  • Extreme pressure protection
  • Protection against shock loading, thus extending bearing life
  • Good high temperature stability to continuous operating temperatures of 250°F

Texaco Miltex EP is a water resistant, extreme pressure grease designed for use in heavy duty industrial equipment, such as steel mill operations.

It is manufactured using highly refined, select high viscosity index base oils, a lithium soap, and a specifically selected additive package containing extreme pressure additives as well as corrosion and rust inhibitors. It will not corrode steel or nonferrous bearing materials.

Texaco Miltex EP is formulated to:

  • Protect bearings and other metal surfaces from corrosion when exposed to wet conditions.
  • Resist water — Strongly resists being washed out of bearings.
  • Retain consistency under adverse service conditions.
  • Provide outstanding film strength and adhesive properties.
  • Operate effectively over a wide temperature range.

Texaco Miltex EP is recommended for use in heavy duty industrial equipment including manufacturing and steel mill operations.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221972; MSDS Number: 8889

Vendors:
Available Properties
  • Saybolt Viscosity at 100°F, See Note 3.
  • Saybolt Viscosity at 210°F, See Note 3.
  • Kinematic Viscosity at 40°C (104°F), See Note 3.
  • Kinematic Viscosity at 100°C (212°F), See Note 3.
  • Penetration P(0), 1/10 mm, Unworked, 25°C (77°F)
  • Penetration P(60), 1/10 mm, Unknown Amount of Work, 25°C (77°F)
  • Maximum Service Temperature, Air, See Note 2.
  • Minimum Service Temperature, Air, See Note 1.
  • Pour Point, See Note 3.
  • Flash Point, See Note 3.
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.