MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Röhm PLEXIGLAS® Multicolor PMMA  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: Multicolored PLEXIGLAS® is a solid acrylic sheet material consisting of two or three layers. The individual layers can be transparent, translucent or opaquely colored. Combinations of these options are also possible. Our special manufacturing process offers the following variations, among others:
  • one surface with a piano lacquer effect
  • smooth or satin surfaces
  • a transparent intermediate layer
  • a colored intermediate layer
  • individual house colors
Properties: The multicolored PLEXIGLAS® grades naturally offer the proven properties of PLEXIGLAS®, such as:
  • excellent light transmission and brilliance
  • extremely high weather resistance
  • ease of fabrication
  • high surface hardness
  • low weight – half the weight of glass
  • 100% recyclability
  • 11 times the impact strength of glass
Applications:
    Kitchens (niche panels)
  • Living rooms (wall design)
  • Interior design in hotels, restaurants, offices….
  • Exhibition booths, furniture, store fixtures
  • Façade construction
  • Displays
  • Illuminated shelves

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors:
Available Properties
  • Density, ISO 1183
  • Ball Indentation Hardness, ISO 2039-1, H961/30
  • Tensile Strength at Break, DIN EN ISO 527
  • Elongation at Break, DIN EN ISO 527
  • Modulus of Elasticity, DIN EN ISO 527
  • Charpy Impact Unnotched, ISO 179/1 fu
  • Maximum Service Temperature, Air
  • Vicat Softening Point, ISO 306, B50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.