Description: - Flexible, loaded, silicone, rubber, magnetic absorber.
- Excellent attenuation across a wide frequency range.
- Ideally suited for far-field applications that require maximum reflection loss at 2-2.5 GHz.
- High magnetic loss, works well in suppressing resonant cavity modes, isolating signals, and attenuating surface currents.
- Available with pressure sensitive adhesive (PSA).
- Can be water-jet or die cut for custom configurations.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |