Casting methods recommended for this alloy: Centrifugal, Die, Investment, Permanent Mold, Plaster, and Sand.
Applications: Bearings, gears, impellers, rocker arms, valve stems, brush holders, bearing races, small boat propellers.
Classified under: Silicon bronzes and silicon brasses. ASTM B584; formerly ASTM B198-13B
Typical data for separately cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.9%