MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Momentive Performance Materials GE Silicones SCS1200 Acetoxy Silicone Construction Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: GE SCS1200 construction silicone glazing sealant is a one-component, high strength, acetoxy silicone adhesive for structural, butt joint and general purpose glazing applications. The material is supplied as a paste, which cures into a durable rubber when exposed to atmospheric moisture.

Features: Silicone Durability, Fast Cure Time, Primerless Adhesion, High Tensile Strength, ±25% Movement Capacity, Stable Consistency (uncured), Cured Thermal Stability, Low Sag or Slump.

Applications: SCS1200 construction silicone glazing sealant is a candidate to consider in structural glazing applications. It may be used as a weather seal product for general purpose glazing, butt glazing and for tall glass-stiffened lobby systems. SCS1200 sealant has been successfully tested in protective glazing applications and may be considered a candidate for such applications. SCS1200 sealant may be considered for sealing air conditioning, vents or other wall penetrations; glass block, metal/plastic signs or marine hardware.

Colors: Translucent(SCS1201), White(SCS1202), Black(SCS1203), Aluminum-metallic(SCS1209), Bronze(SCS1297).

Information provided by Momentive Performance Materials.

Vendors:
Available Properties
  • Volatile Organic Compounds (VOC) Content, WPSTM C1454, Uncured
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D412
  • Elongation, Ultimate, ASTM D412
  • Shear Strength, ASTM C961
  • Tear Strength, ASTM D624, Die B.
  • Peel Strength, ASTM C794, 50%RH
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Full cured. Common applications.
  • Cure Time, 1/4" deep section. 50% RH
  • Tack-Free Time, ASTM C679, 50% RH
  • Working Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Momentive Performance Materials (GE Silicones)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.