Notes: 60GF2 is a 10% glass fiber grade of nylon 6 that offers good mechanical performance. Availability: Europe; North America Features: High Stiffness; High Strength; Low Density Fillers/Reinforcement: Glass Fiber, 10% Filler by Weight Processing Method: Injection Molding Information provided by Teknor Apex |