MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
DuPont Elvax® CM3326 Ethylene Vinyl Acetate  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: DuPont™ Elvax® CM3326 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.

Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low melt indices. Due to the high VA content, the polymers have low crystallinity and are relatively polar. Combined with high molecular weight (low MI), the polymers are almost "rubbery" in nature. These polymers can be blended with hydrocarbon waxes to give blends with unusual properties. The blends are mostly wax so they have excellent barrier properties to water as measured by MVTR. They are also relatively high in viscosity, due to the low MI of the polymer, so the blends have good physical properties. The high VA level means that these polymers are also soluble in organic solvents. The low MI gives them good heat resistance and this can be seen in the high Ring and Ball numbers. These polymers also can be used in other end-use markets that need the combination of high vinyl acetate and high molecular weight. One drawback is that the polymers are higher in gel than the standard grades of Elvax® to they cannot be used in some film markets.

Applications:Elvax® CM576 resins can be used for the following applications: adhesives, sealants, and wax blends.

Information provided by DuPont™

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors:
Available Properties
  • Density, ASTM D792-ISO 1183
  • Vinyl Acetate Content
  • Melt Flow, ASTM D1238, ISO 1133
  • Hardness, Shore A, ASTM D2240-ISO 868
  • Tensile Strength at Break, ASTM D638 ISO 527-2
  • Elongation at Break, ASTM D638 ISO 527-2
  • Melting Point, ASTM D3418, Freezing Point
  • Melting Point, ASTM D3417- ISO 3146
  • Ring & Ball Softening Point, ASTM E28
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Packaging and Industrial Polymers

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.