Moplen EP542T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP542T is a block copolymer selected by customers for use in injection molding of automotive parts and thin-walled packaging, parts of electrical appliances, housewares like chopping board, etc. Moplen EP542T resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Product Features: Optimized balance of stiffness and impact/High flowability/FDA Approval Typical Applications: TWIM/Chopping board/Parts of electrical appliances/Automotives part Information provided by PolyMirae |