Cure: Room temperature or Heat cure
Application: Potting, Encapsulant
Loctite Stycast 2651-40 W1 epoxy encapsulant is designed for general purpose applications and has excellent adhesion to a wide variety of substrates. When fully cured, the material is readily machined with carbide tools.
Loctite Stycast 2651-40 W1 can be used with a variety of catalysts.
CATALYST DESCRIPTION
Loctite CAT 27-1 provides the following product characteristics:
Cure: Heat cure