Description: Unreinforced polyamide 6, very high viscosity, for extrusion. Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, sheets, pipes. All the semi-finished products can be machined without special treatment, such as: Precision gears, bolts, etc. This product is available in natural. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |