  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP21DP12 Two component urethane modified epoxy for bonding, sealing and potting
Categories: Polymer; Thermoset; Epoxy

Material Notes: Master Bond EP21DP12 is a two component, urethane modified epoxy for bonding, sealing and potting applications. It has a forgiving 2 to 1 mix ratio by weight along with a conveniently extended working life. This system cures at ambient temperatures or more readily at elevated temperatures. The optimum cure schedule is overnight at room temperature followed by 2 to 3 hours at 135-150°F. It is 100% reactive and does not contain any solvents or diluents. Also, it contains an air release agent which allows for facilitated degassing. EP21DP12 bonds well to a wide variety of substrates such as metals, glass, ceramics and many types of rubbers and plastics. The urethane component allows the system to withstand temperature cycling as well as thermal and mechanical shocks more readily than typical epoxies. EP21DP12 has good resistance to water, oils and fuels. It is a dependable electrically isolating material. It generates relatively low exotherm in comparison to other systems and is appropriate for potting applications up to 2-2.5 inches thick. The service temperature range is -100°F to +250°F. It is available in red, green, blue, black and white for identification or cosmetic purposes. This epoxy is an interesting option for bonding and potting where a toughened system along with a distinctive color are desirable features.

Product Advantages:

  • Convenient 2 to 1 mix ratio by weight
  • Long open time
  • Withstands thermal cycling and mechanical shock
  • Good abrasion resistance
  • Available in cans or with a gun type dispensing systems
Key Features:
  • Excellent toughness
  • Convenient processing
  • Can withstand rigorous thermal cycling
  • Available in several colors

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Optimal: overnight at 75°F plus 2-3 hours at 135-165°F
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Working Life, 100 gram batch
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.