MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
AISI 1050 Steel, water quenched from 830°C (1525°F), 540°C (1000°F) temper, 100 mm (4 in.) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: The composition listed applies only to structural shapes, plates, strip, and welded tubing. Semifinished products for forging, hot-rolled and cold-finished bars, wire rods, and seamless tubing have a carbon range of 0.48 - 0.55%.

Key Words: UNS G10500, AMS 5085, ASTM A29, ASTM A510, ASTM A519, ASTM A576, ASTM A682, DIN 1.1210, JIS S 53 C, JIS S 55 C, FED QQ-S-635 (C1050), FED QQ-S-700 (C1050), MIL SPEC MIL-S-16974, SAE J403, SAE J412, SAE J414
Vendors:
Available Properties
  • Density, Typical for steels.
  • Hardness, Brinell
  • Hardness, Knoop, Converted from Brinell
  • Hardness, Rockwell B, Converted from Brinell
  • Hardness, Rockwell C, Converted from Brinell
  • Hardness, Vickers, Converted from Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Reduction of Area
  • Modulus of Elasticity, Typical for steel
  • Bulk Modulus, Typical for steels.
  • Poissons Ratio, Typical For Steel
  • Shear Modulus, Typical for steels.
  • Izod Impact, annealed at 790°C (1450°F)
  • Izod Impact, normalized at 900°C (1650°F)
  • Izod Impact, as rolled
  • Electrical Resistivity, annealed specimen
  • Electrical Resistivity, annealed specimen
  • Electrical Resistivity, annealed specimen
  • CTE, linear, Typical steel
  • CTE, linear, Typical for steel
  • CTE, linear, Typical for steel
  • Specific Heat Capacity, annealed
  • Thermal Conductivity, Typical steel
  • Carbon, C
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Phosphorus, P
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.