INNOBATCH® PPH 3260 is a 60% chalk-filled polypropylene homopolymer based masterbatch. This grade is available in natural form. These products that are offered under the brand name INNOBATCH® are recommended for the area of packaging materials, but they can be used for manufacturing household appliances and outdoor furniture and for other purposes as well. The raw material having filler content is a semi-finished product from a user point of view; this allows the user to determine the optimal feeding rate during the processing operation. Information provided by INNO-COMP |