MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Tin Bronze, UNS C90500, Copper Casting Alloy, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Effect of Section Size; Medium – Casting Yield, Gassing, Fluidity, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability - Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Clamps; Heavy Construction Equipment; Connectors; Nuts; Bearings; Bushings; Expansion Bearings; Finishing Dies for Wood Pulp Industry; Gear Blanks; Gears; Piston Rings; Pump Bodies; Pump Impellers; Seal Rings; Valve Bodies; Valves; Worm Gears; Steam Fittings; Water Conditioners

Applicable Specifications: As Centrifugal Cast – Castings SAE J462; Castings SAE J461, Castings ASTM B271/B271M, Castings AMS 4845; As Continuous Cast – Castings ASTM B505/B505M, Castings SAE J462, Castings SAE J461; As Sand Cast – Castings SAE J461, Castings AMS 4845, Castings SAE J462, Castings ASTM B584, Castings ASTM B22/B22M, Castings ASTM B763/B763M; Ingot - ASTM B30; Precision Cast – Castings MILITARY MIL-C-11866

Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, for Standard
  • Tensile Strength, Typical
  • Tensile Strength, Yield, for Standard, 0.5% Ext
  • Tensile Strength, Yield, Typical, 0.5% Ext
  • Elongation at Break, for Standard
  • Elongation at Break, Typical
  • Tensile Modulus
  • Compressive Strength, 0.01 in. set/in.
  • Fatigue Strength
  • Machinability
  • Izod Impact
  • Electrical Resistivity, 11% IACS
  • Magnetic Permeability
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Shrinkage, Patternmaker's Shrinkage (3/16 in./ft.)
  • Processing Temperature, Stress Relief
  • Aluminum, Al
  • Antimony, Sb
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.