Dutral® TER 4436 is an Ethylene - Propylene - Diene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process. Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® TER 4436 is a semi-crystalline, very high molecular weight terpolymer of medium diene content, extended with 40% paraffinic oil. It is characterized by high loading capacity, good green strength and can be used to obtain low hardness final articles. Dutral® TER 4436 based compounds present high dimensional stability and good curing rate. Main Applications: Automotive, mechanical goods, appliances, TPV. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |